About wet marks or wax marks under coating after paint spraying:

Source:本站    Release time:2022-10-19 15:05:12    Click volume:

About wet marks or wax marks under coating after paint spraying:

 

1. What are the wax marks under wet printing or coating: from the surface of the paint layer, the outline of the contaminated area on the bottom layer can be seen, or matt spots of various shapes appear.

 

2. Cause:

 

The underlying surface is not thoroughly cleaned before painting, for example, grease or wax is not completely removed.

 

The previous paint layer is not dried or the defects of the old paint layer are not removed.

 

The previous paint layer is incompatible with the re-sprayed paint layer.

 

 

3. Correction method:

 

If the wet print is more obvious, it should be sanded off the paint layer and re-sprayed.